composition |
Parameter |
|
Pure lead |
Pb-99.99% |
|
Lead-antimony alloy |
Sb-0.3-0.4% |
|
Lead-stannum-antimony alloy |
Sn-0.4%; Sb-0.2% |
|
Lead-antimony-copper alloy |
Sb-0.4%; Cu-0.04% |
|
Lead-stannum-cadmium alloy |
Sn-0.2%; Cd-0.075% |
|
No. |
Item |
Unit |
Qty |
|
1 |
Active Loading ingot unit with rollers |
set |
1 |
|
2 |
118T melting furnace(installation in parallel ) |
set |
2 |
|
3 |
Ω pipe |
pc |
1 |
|
4 |
Host machine of ¢200/5 lead extruder |
set |
1 |
|
5 |
Gear lubricant oil system |
set |
1 |
|
6 |
Internal Water circulating & cooling system |
set |
1 |
|
7 |
Rear water cooling system |
set |
1 |
|
8 |
Vertical single guide roller frame for inlet and outlet cables |
pc |
2 |
|
9 |
Flowage control unit(shift by manual or automatic control) |
set |
1 |
|
10 |
Electrical control system |
set |
1 |
cable dia. scope Φ36~Φ152mm
Lead sheathing scope: Φ40~Φ160mm
Extruding Output:
|
Lead composition |
Screw speed (rpm) |
Extruded output (kg/min) |
|
Pure lead |
6~12rpm |
30~45Kg/min |
|
Soft alloy lead |
6~9rpm |
15~30Kg/min |
|
Hard alloy lead |
6~9rpm |
13~24kg/min |
Thickness of lead layer: 1.6~4.6mm
Lead layer tolerance: ± 0.2~0.5mm